Thermally Conductive Silicone Potting Compounds
∎Product Description
SI8230 is a two-component silicone based thermal conductive potting adhesive. It has a good fluidity after mixing, can vulcanize to a deep layer in room temperature. The operation time can be adjusted according to the temperature. Used to potting protection of varied heat dissipation and temperature resistance components. Fully compliant with RoHS and SVHC REACH standards.
.
∎Typical Applications
●Used for encapsulation of various modules, automotive module, LED Power driver modules, Solar panel junction box, EV charging column module, Lithium battery pack, Capacitor banks, Magnetic induction coils, Power inverters, etc.
∎Key Features
- Two-part 1:1 mixture addition type silicone adhesive
- Low hardening shrinkage
- Excellent electrical insulation in high temperature and stability
- Good waterproof and moisture resistance
- Excellent flame-resistance, UL No: E340199
∎Packing Specification
●SI8230W white thermal conductivity silicone potting sealant
●SI8230B black thermal conductivity silicone potting sealant
●SI8230G gray thermal conductivity silicone potting sealant
- Part A:20 kg/plastic drum
Part B:20 kg/plastic drum
- Part A:250 kg/plastic drum
Plat B:250 kg/plastic drum
∎Transport &Storage
● When stored at or below 35°C in the original unopened containers, this product has a usable life of 12 months from the date of production. Sampling test is necessary for products which exceed shelf life before taking use. During storage may have little settlement stratification, stirring evenly when use, does not affect performance.
It’s non-dangerous goods, can be transported as normal chemicals, CAUTION leakage during transport.
.∎Directions for Use
Mixing uniformity in the packing before using, as there’s part of filler sedimentation happens during storage.
Mix Part A and Part B by 1:1 mass ratio, after evenly mixed, pouring directly into the components or modules as per requirements. It’s recommended to slowly pour along the walls of the implements, so as to reduce the bubbles happens.
Still the potted component to let out the bubbles. Can be cured by heat, about 30 minutes in 80°C. If cured under room temperature, about 4 hours.
- Vacuum defoaming can improve the performance of cured product.
- Seal the remaining products tightly after use.
- Low temperature will slow the curing speed, overheating will lead to curing speed too fast. Keep the constant temperature in workshop is recommended.
- It's hard for SI8230 to cure if contact with sulfur, amine, organotin and unsaturated hydrocarbon plasticizer. Common substances like rosin, natural rubber. For these should do test before application.
∎Attention of operation
●Keep away from Children
●Avoid contact with eyes and skin. If contact with your skin, scrub first with soap water or alcohol, then rinse with water. If contact with your eyes, rinse with plenty of water, and seek medical treatment immediately.
● It is forbidden to build on the surface of the wet substrate.
Thermally Conductive Silicone Potting Compounds
TESTING ITEM
ESTING STANDARD
Part A
Part B
Color
Visual inspection
White / black viscous liquid
White viscous liquid
Viscosity, cps , 25℃
GB/T 10247-2008
2500±500
2300±500
Density,,g/cm3, 25℃
GB/T 15223-1994
1.52±0.03
1.52±0.03
Mixture ratio
Weight Ratio
A:B = 100:100
Viscosity of mixture,4#rotor,cps , 25℃
GB/T 10247-2008
2500±500
Operation time,mins , 25℃
GB/T 10247-2008
50±10
Tack free, mins, 25℃
GB/T 10247-2008
90±20
Cure condition
GB/T 10247-2008
25℃/3-5 hr or 80℃/ 30mins
Characteristics after curing
Cured appearance
Visual inspection
Gray, white or black elastomer
Hardness, Shore A
GB/T 531-2008
55±5
Thermal conductivity,W/mK
GB/T 10297-1998
0. 65±0.03
Linear expansion,K-1,ppm
HGT 2625-1994
230
Dielectric strength ,kV/mm, 25℃
GB/T 1695-2005
≥15
Volume resistance,DC 500V, Ω·CM
GB/T 1692-92
1.1×1015
Loss factor(1 MHz)
GB/T 1693-2007
0.009
Dielectric constant(1 MHz)
GB/T 1693-2007
3.00
Application temperature, ℃
GBT 20028-2005
- 60 ∽ 200
Flame resistance
UL-94
V-0